Conseal Touch-Up One-component Physically Drying Acrylic Coating is an acrylic coating used as a topcoat. In the industrial protective coatings sector: recommended for refineries, power stations, bridges and buildings. A one-component physically drying acrylic coating. Parameters on this page: volume solids 49 ± 2%; dry film thickness 75–120 µm; theoretical spreading rate 6.5–4.1 m²/L. Comparable products from the same brand: Hardtop CA Two-component Acrylic Topcoat, Hardtop One Moisture-curing Acrylic Polysiloxane Topcoat, Hardtop Pro SG Acrylic Polysiloxane Topcoat SG.
Source: JOTUN original technical data sheet (TDS) 'Conseal Touch-Up One-component Physically Drying Acrylic Coating'. Spreading rate and other values converted from the TDS; for reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 49 ± 2% |
|---|---|
| Dry Film Thickness | 75–120 µm |
| Theoretical Spreading Rate | 6.5–4.1 m²/L |
| VOC | 463 g/L |
| Density / Specific Gravity | 1.2 kg/L |
| Number of Components | One-component |
| Flash Point | 25 °C |
| Thinner | JOTUN Thinner No. 7 |
| Gloss | Matt (0–35) |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
A one-component physically drying acrylic coating. Its film has a matt finish. It is a high-build product. Fast drying. Can be applied directly to metal. Used as a topcoat in atmospheric environments. Can be applied at surface temperatures below 0 °C.
Industrial protective coatings:
Recommended for refineries, power stations, bridges and buildings. Widely suitable for industrial structures.
Others
Grain certificate issued by the Newcastle (UK) occupational health authority. Other certificates and approvals are available on request.
Tinted according to the colour chart and using the industrial tinting system (MCI)
| Property | Test / Standard | Description |
| Volume Solids | ISO 3233 | 49± 2 % |
| Gloss (GU 60°) | ISO 2813 | Matt (0–35) |
| Flash Point | ISO 3679 Method 1 | 25 °C |
| Density | Theoretical Value | 1.2 kg/L |
| VOC — USA / Hong Kong | US EPA Method 24 (test value) (CARB (SCM) 2007, SCAQMD Rule 1113, Hong Kong) | 463 g/L |
| VOC — EU | IED (2010/75/EU) (theoretical value) | 470 g/L |
The data listed are based on factory batch production and may vary slightly with colour.
| Gloss description | According to JOTUN's definition of functional coatings |
|---|
Typical recommended specification range
| Dry Film Thickness | 75–120 µm |
| Wet Film Thickness | 150–245 µm |
| Theoretical Spreading Rate | 6.5–4.1 m²/L |
Surface Preparation
| Substrate | Minimum | Recommended |
| Coated surface | A clean, dry and sound compatible primer. | |
| Carbon Steel | St 2 (ISO 8501-1) | Sa 2½ (ISO 8501-1) |
| Shop-primed Steel | Clean, dry and intact shop primer (compliant with ISO 12944-4 clause 5.4). | Sa 2 (ISO 8501-1) |
| Aluminium | The surface should be abraded by hand or machine using a non-metallic abrasive, fibre discs or abrasive paper to produce scratch marks. | Cleanliness conforming to Sa 1 (ISO 8501-1). |
| Galvanised steel | The surface should be clean, dry and have a suitable profile | Sweep blast with a non-metallic abrasive to produce a clean, |
| ° | a rough and uniform surface. | |
This product may be applied by the following methods
| Spray: | For airless spray, thin the coating 5–10%. |
| Brush: | Use a suitable brush. Take care to achieve the specified dry film thickness. |
| Roller: | May be used, but not recommended for the first coat on bare metal. Ensure the specified dry film thickness is achieved. |
One-component
| Thinner | JOTUN Thinner No. 7 |
|---|
| Nozzle tip size (inch/1000): | 17-23 |
| Nozzle pressure (minimum): | 150 bar/2100 psi |
| Substrate Temperature | -5 °C | 0 °C | 5 °C | 10 °C | 23 °C | 40 °C |
| Touch Dry | 30 min | 20 min | 17 min | 15 min | 10 min | |
| Walk-on Dry | 20 h | 17 h | 11 h | 10 h | 6 h | |
| Minimum recoat interval | 4 h | 3 h | 2.5 h | 2 h | 1.5 h | |
For the maximum recoat interval, refer to the Application Guide (AG) for this product.
Drying and curing times are determined based on temperature and relative humidity below 85%, with dry film thickness within the average range.
| Touch Dry | The state at which light finger pressure leaves no mark or stickiness. |
|---|---|
| Walk-on Dry | The minimum time after which the coating allows normal foot traffic without leaving permanent footprints, marks or other physical damage. |
Minimum recoat interval after drying: the recommended minimum interval before applying the next coat.
Temperature
| Continuous | Peak | |
| Drying, atmospheric | 60 °C | - |
At elevated temperatures, the dry film gradually softens. Establish correct handling and stacking procedures according to the environmental conditions. Protective performance is unaffected.
Depending on the actual exposure conditions in service, this product may be used with various primers and topcoats. Some reference systems are listed below. For specific systems, contact JOTUN.
| Previous coat: | Acrylic, epoxy, zinc-containing epoxy, shop primer |
| Subsequent coat: | Acrylic |
| Volume | Container Size | |
| (L) | ||
| Conseal Touch-Up | 5 / 20 | |
The packaging sizes above are typical reference sizes for factory batch production. Due to regional regulatory differences, packaging sizes and capacities may vary by region.
Store in accordance with national regulations. Keep in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.
Conseal Touch-Up, 48 months
In some markets, the stated shelf life may be shortened to comply with local legal requirements. The above is the minimum shelf life; thereafter, testing is required to confirm quality remains acceptable.
For professional use only. Applicators and workers must be trained, experienced, capable and equipped to mix, stir and apply the coating correctly in accordance with JOTUN's technical documents. Applicators and workers must wear appropriate personal protective equipment when using this product. This guidance is provided based on current product knowledge. Any proposed modification to suit site conditions must be approved by the responsible JOTUN representative before use.
Read the safety warnings on the container packaging. Use in well-ventilated conditions. Avoid inhaling spray mist and avoid skin contact. In case of accidental splashes on skin, wash immediately with a suitable cleaner, soap and water. In case of eye contact, rinse thoroughly with water and seek medical attention immediately.
When used primarily as a primer or antifouling coating, products may show slight colour variation from batch to batch. Such products, and epoxy products used as topcoats, may chalk when exposed to sunlight.
Gloss and colour retention of topcoats depend on the colour type, the surrounding environment such as temperature and UV intensity, application quality and product type. Contact your local JOTUN office for further information.
The information in this datasheet is based entirely on knowledge gained in our laboratory and in practice. JOTUN products are regarded as semi-finished products, and their use is generally beyond our control. JOTUN therefore guarantees only the quality of the product itself. To comply with local regulations, the product may be adjusted, and we reserve the right to modify the datasheet without further notice.
Users should consult JOTUN for specific guidance on the suitability of the product for their requirements and applications.
In case of any discrepancy between language versions, the English (UK) version shall prevail.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.