THERISO UNDERCOAT is a thermal insulation coating in the epoxy system. For structures needing heat-insulation properties. Used as an insulating intermediate coat for equipment requiring thermal insulation, such as tanks, special containers and warehouses. A polyamide-cured modified epoxy thermal insulation coating. Parameters on this page: volume solids 53 ± 2%, theoretical spreading rate 0.256 kg/m²/100 µm, number of components two. Comparable products from the same brand: EPOFEND GLASS 30 Epoxy Glass Flake 30, EPOFEND ZINC 60 Epoxy Zinc-rich Primer 60, EPOMARINE BTD Epoxy Topcoat.
Source: KANSAI original technical data sheet (TDS) "THERISO UNDERCOAT"; spreading rate and other values are converted from TDS parameters and are for selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 53 ± 2% |
|---|---|
| Dry Film Thickness | 50–100 µm/coat |
| Theoretical Spreading Rate | 0.256 kg/m²/100 µm |
| VOC | — |
| Density / Specific Gravity | — |
| Number of Components | Two-component |
| Flash Point | Above 13 °C |
| Thinner | Epoxy Thinner 20# |
| Mixing Ratio | Base/Hardener=9/1(by weight) |
| THERISO UNDERCOAT | Thermal insulation intermediate coat |
|---|
A polyamide cured modified epoxy heat protection coating.
As heat insulation undercoat can be used in storage tank, special container, storehouse and other steel
Goof heat protection effect
| Color | White or light Grey |
|---|---|
| Colour | White/light grey |
| Volume Solids | 53±2% |
| Flash Point | Greater than 13°C |
| Flash Point | Above 13 °C |
| Film thickness | Dry : 50-100µm /coat Wet : 95-191µm /coat |
| Applied film thickness | Dry film: 50–100 µm/coat; wet film: 95–190 µm/coat |
| Theoretical Coverage | 0.256 kg/m²/100µm |
| Theoretical Spreading Rate | 0.256 kg/m²/100 µm |
Practical coverage depending on surface conditions, environment, applications, etc.
| Application Temperature | 5°C-40°C |
|---|---|
| Mixing | Combine Base with Hardener, mix thoroughly with power agitator |
| Mixing | Mix the base and curing agent and stir thoroughly with a power tool |
| Mixing Ratio | Base/Hardener=9/1(by weight) |
| Mixing ratio | Base : curing agent = 9:1 (by weight) |
| Pot Life | 5°C | 10°C | 20°C | 30°C |
| Pot life | 16hrs | 12hrs | 8hrs | 6hrs |
| Application Methods | Airless spray, air spray, brush and roller |
|---|---|
| Application Methods | Airless spray, air spray, brush and roller. Air spray: airless spray. Thinning ratio 5–15% by volume (by volume). Brush/roller. Thinning ratio 0–5% by volume (by volume). |
| Thinner | Epomarine Thinner 20# |
| Thinner | Epoxy Thinner 20# |
| Drying time & | Temperature | 5°C | 10°C | 20°C | 30°C | |
| Overcoating interval | Surface dry | Touch dry | 6hrs | 3hrs | 1hrs | 0.5hrs |
| Drying time & recoat interval | Touch dry | Semi-hard dry | 48hrs | 24hrs | 16hrs | 12hrs |
| Min. interval | Minimum recoat interval | 24hrs | 16hrs | 12hrs | ||
| Max. interval | Maximum recoat interval | 7 | 7 | |||
| Preceding coat | SD Zinc 500,Epomarine EX-500, or according to the coating systems of COSCO Kansai |
|---|---|
| Suitable for undercoating | Epoxy zinc-rich, epoxy, or refer to COSCO KANSAI coating system |
PU Finish RT-30 , or according to the coating systems of COSCO Kansai
| Typical topcoat; suitable overcoat | Polyurethane thermal insulation topcoat, or refer to COSCO KANSAI coating system |
|---|
Store in dry, cool condition and away from sources of heat and ignition. Containers must be kept
tightly closed.
| Shelf life | 12 months from date of production (25°C) |
|---|---|
| Shelf life | 12 months from date of production (25 °C) |
The information given on this sheet is to the best of our knowledge and accurate at the time of issuing.
Since conditions of use are beyond the manufacturer’s control, information contained herein is without warranty, implied or otherwise, and the suitability of the material for the use contemplated is the sole responsibility of the buyer. The information contained on this data sheet is subject to modification at any time due to our policy of modification and product development. Please check this date sheet is current prior to using the product.
The information provided in this data sheet is, to the best of our knowledge, the most complete and accurate information currently available. As the conditions of product use are beyond our control, this information carries no warranty, and we are responsible to the buyer only in the selection of the product. As our products and production processes are continuously developed, the content of this data sheet is subject to change at any time, and all information herein is subject to our confirmation. Confirm that the data sheet in hand is the latest version before using the product.
| Issued Date | 2019 |
|---|
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.