HEMPEL Fluorocarbon Topcoat 55LCN is a fluorocarbon paint used as a topcoat. It can be used as a protective and decorative topcoat on steel structures and cement surfaces requiring high gloss retention and colour retention, maintaining long-term appearance even in severe pollution environments. HEMPEL Fluorocarbon Topcoat 55LCN is a two-component ambient-curing fluorocarbon coating used as a long-life high-performance topcoat, with good gloss retention and colour retention. Parameters on this page: volume solids 55 ± 2%, dry film thickness 50 µm, theoretical spreading rate 11 m²/L. Comparable products from the same brand: HEMPEL High-solids Fluorocarbon Topcoat 830, HEMPEL Acrylic High-build Topcoat 460CN, HEMPEL Acrylic Enamel 5636E.
Parameter source: HEMPEL original Technical Data Sheet (TDS) 'HEMPEL Fluorocarbon Topcoat 55LCN'; values such as spreading rate are converted from TDS parameters and are for product selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 55 ± 2% |
|---|---|
| Dry Film Thickness | 50 µm |
| Theoretical Spreading Rate | 11 m²/L |
| VOC | 443 g/L (China) |
| Density / Specific Gravity | 1.4 kg/L |
| Number of Components | Two-component |
| Flash Point | 27°C |
| Colour / Appearance | White 10000 ** |
| Gloss | Semi-gloss |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
HEMPEL Fluorocarbon Topcoat 55LCN is a two-component ambient-curing fluorocarbon coating used as a long-life high-performance topcoat, with good gloss retention and colour retention. It meets the technical requirements of JT/T722-2008, the standard for anti-corrosion coating of steel structures for highway bridges.
Can be used as a protective and decorative topcoat on steel structures and cement surfaces requiring high gloss retention and colour retention, maintaining long-term appearance even in severe pollution environments.
| Product safety | Flash point 27 °C |
|---|
| Regulations | Value |
| European Union | 443 g/L |
| USA (coatings) | 443 g/L |
| USA (regulatory) | 443 g/L |
| China | 443 g/L |
Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. VOC values may vary with colour; refer to Section 9 of the Safety Data Sheet. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.
Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.
For professional use only.
| Product code | 55LCN |
|---|---|
| Product components | Base 55LC9 |
Curing Agent 955CN
| Standard colour* / code | White 10000 ** |
|---|---|
| Gloss | Semi-gloss |
| Volume solids | 55 ± 2% |
| density | 1.4 kg/L |
| Recommended dry film thickness | 50 µm |
_______________________________
| Aluminium colour / code | Aluminium Grey 19000 *** |
|---|
Refer to the Hempel Guide for Aluminium-containing Coatings.
| Volume solids | 49 ± 2% |
|---|---|
| density | 1.2 kg/L |
| Recommended dry film thickness | 50 µm |
For further details, refer to the separate Hempel document Surface Preparation Guide.
Base 55LC9 : Hardener 955CN (92 : 8 by volume)
Stir thoroughly before use.
Hempel's Thinner 014CN
| Product temperature | 10°C | 20°C | 30°C |
| Pot Life | 3 h | 2 h | 1½ h |
| Tools | Maximum thinning volume | Application parameters |
| Airless Spray | 5% | Nozzle pressure: 15 MPa; nozzle tip size: 0.33–0.53 mm |
| Air Spray | 5% | Not applicable. |
Additional thinning may be required to reduce dry spray at high temperatures. Additional thinning may be required at low paint temperatures; this will result in lower film build and slower drying. Do not thin components separately; thinning after mixing is permitted. Spray parameters are indicative and may be adjusted to site conditions. Pressure values apply to material at 20°C. (*Consult the company representative for other application methods.)
| Specification range | Low | High | Recommended |
| Dry Film Thickness | 30 µm | 70 µm | 50 µm |
| Wet Film Thickness | 50 µm | 125 µm | 90 µm |
| Theoretical Spreading Rate | 18 m²/L | 7.8 m²/L | 11 m²/L |
Depending on the end use and service area, the product may be specified at film thicknesses other than those indicated.
This will change the application rate, drying and curing times and recoat interval. Avoid excessive film thickness to achieve the desired performance. Actual consumption factors may vary with application conditions, equipment and workmanship. Checking paint consumption against area improves film thickness control.
| Surface temperature | 0°C | 10°C | 20°C | 30°C |
| Touch Dry | 36 h | 16 | 8 | 6 |
| Surface Dry | - h | - | 2½ | - |
| Fully cured | - days | - | 7 | - |
Measured at 50 µm dry film thickness under standard conditions; see Hempel's explanatory notes. To determine the drying state, refer to the Application Specification COP FP1401-1 (drying test for high film thickness)
Hempel's specifications supersede all guidance shown in the recoat table.
| Product name | 10°C | 20°C | 30°C | 40°C | |
| Atmospheric, mild | |||||
|---|---|---|---|---|---|
| HEMPEL's Fluorocarbon Topcoat 55LCN | Minimum | 9 h | 6 h | 3 h | 100 min |
| Maximum | Extended | ||||
| Atmospheric, moderate | |||||
| HEMPEL's Fluorocarbon Topcoat 55LCN | Minimum | 9 h | 6 h | 3 h | 100 min |
| Maximum | Extended | ||||
| Atmospheric, severe | |||||
| HEMPEL's Fluorocarbon Topcoat 55LCN | Minimum | 9 h | 6 h | 3 h | 100 min |
| Maximum | Extended | ||||
For products of the same generic chemical composition, recoat times are for reference only.
For further information, refer to Hempel's specifications.
- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.
- Avoid exposing touch-up areas, full coats and intercoat intervals to high humidity during application.
| Number | Document description | Location/Notes |
| 3. | PDS | This document |
datasheet, which is also available for download at www.hempel.com.
| Ambient temperature | 25°C |
| Binder | 12 months |
| Curing agent | 24 months |
Shelf life is the period from the date of manufacture while the product is stored in its original, unopened containers. After this period, the product quality shall be re-tested. Always check the best-before or expiry date on the label.
For more information, refer to the Hempel website hempel.com or the local Hempel website:
- General Application Guide. This Product Data Sheet ('PDS') relates to the supplied product ('Product') and its content is updated from time to time. The buyer/applicator shall therefore refer to the PDS supplied with the relevant product batch (not earlier versions). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, statements and/or guides shown below; such documents may also be downloaded from the 'Products' page of the Hempel website (www.hempel.com) (hereinafter 'Supplementary Documents'):
| 1. | Technical declaration | Provides one-off specific advice for the requirements of a specific project |
| 2. | Specifications | Issued for specific projects only |
| 4. | Explanatory notes to the PDS | Available for download at www.hempel.com, containing information related to product test parameters |
| 5. | Application guide | If available, provided at www.hempel.com |
| 6. | General technical guidelines (e.g. application and surface preparation) |
If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.