HEMPEL Waterborne Epoxy Zinc-Rich Primer 530 is a zinc-rich primer, in the waterborne coating system. Used as an anticorrosive primer or zinc-rich epoxy shop primer in waterborne container coating systems under medium to severe atmospheric exposure. The dry film zinc content reaches 80 ± 2% (by weight). Parameters on this page: volume solids 47 ± 2%, dry film thickness 20 µm, theoretical spreading rate 23 m²/L. Comparable models from the same brand: HEMPEL Epoxy Zinc-Rich Primer, HEMPEL Vanguard Epoxy Zinc-Rich Primer 550, HEMPEL Vanguard Epoxy Zinc-Rich Primer 650.
Parameter source: HEMPEL original technical data sheet (TDS) for HEMPEL Waterborne Epoxy Zinc-Rich Primer 530; spreading rate and other values are converted from TDS parameters and provided for product selection reference only.
The above content is compiled from the manufacturer's datasheet and this site's parameter tables. For selection, coating systems and lead times, pleaseContact Usfor confirmation.
This page carries the full TDS for this product, translated from the manufacturer's original document. No file download is needed; for an original-language copy, send an enquiry.
| Volume Solids | 47 ± 2% |
|---|---|
| Dry Film Thickness | 20 µm |
| Theoretical Spreading Rate | 23 m²/L |
| VOC | 221 g/L (China) |
| Density / Specific Gravity | 2.2 kg/L |
| Number of Components | Two-component |
| Flash Point | 37°C |
| Colour / Appearance | Grey 19840 * |
| Pot Life | 3½ h |
For more Q&A on selection, application, acceptance and defect diagnosis, seeFAQsection.
HEMPEL Waterborne Epoxy Zinc-Rich Primer 530 is a two-component, waterborne, fast-drying epoxy zinc-rich coating that cures to a good anticorrosive coating, protecting locally mechanically damaged areas through cathodic protection. The dry film zinc content reaches 80 ± 2% (by weight).
Used as an anticorrosive primer or zinc-rich epoxy shop primer in waterborne container coating systems under medium to severe atmospheric exposure.
| Product safety | Flash point 37 °C |
|---|
| Regulations | Value |
| European Union | 221 g/L |
| USA (coatings) | 219 g/L |
| USA (regulatory) | 331 g/L |
| China | 221 g/L |
Subject to specific legislation; see the explanatory notes on the Hempel website hempel.com or your local Hempel website. This product complies with the VOC requirements of national mandatory or recommended standards; consult the company representative for details.
Handle with care. Before and during use, observe the safety labels on the packaging and paint containers and comply with all local and national safety regulations. Consult the Hempel Safety Data Sheet and Product Data Sheet for the product at all times.
For professional use only.
| Product code | 1836C |
|---|---|
| Product components | Base 1836Q |
Curing agent 9846C
| Standard colour / code | Grey 19840 * |
|---|---|
| Volume solids | 47 ± 2% |
| density | 2.2 kg/L |
| Recommended dry film thickness | 20 µm |
For further details, refer to the separate Hempel document Surface Preparation Guide.
Base 1836Q : Curing agent 9846C (1 : 1 by volume)
Products containing floating or settling particles/pigments require continuous stirring during application; this is especially important when heavily thinned.
Thinner
Fresh water
Cleaning solvent
| Product temperature | 20°C |
|---|---|
| Pot Life | 3½ h |
| Tools | Application parameters |
|---|---|
| Airless Spray | Tip size: 0.38–0.43 mm |
| Brush | Not applicable. |
If brush or roller application is used, several coats may be required to achieve the specified dry film thickness. Spray parameters are indicative and may be adjusted to suit site conditions. Pressure figures apply to the material at 20 °C. (*For other application methods, consult the company representative.)
| Specification range | Low | High | Recommended |
| Dry Film Thickness | 10 µm | 50 µm | 20 µm |
| Wet Film Thickness | 21 µm | 107 µm | 43 µm |
| Theoretical Spreading Rate | 47 m²/L | 9.3 m²/L | 23 m²/L |
Over-thickness must be strictly controlled; locally, 50 µm [2.0 mil] DFT must never be exceeded. In the case of surface irregularities, particular care is recommended to avoid over-application.
| Surface temperature | 20°C | 40°C | 60°C | 70°C |
| Touch Dry | 15 min | 12 | 9 | 6 |
| Through dry | 12 h | - | ||
Dry film thickness 20 µm measured under standard conditions; see Hempel's explanatory notes for details.
Hempel's specifications supersede all guidance shown in the recoat table.
| Product name | 10°C | 20°C | 30°C | 40°C | |
| Atmospheric, mild | |||||
|---|---|---|---|---|---|
| HEMPEL's Water-borne Epoxy Modified Finish 320 | Minimum | 15 h | 6 h | 3 h | 110 min |
| Maximum | Extendable* | ||||
| Atmospheric, moderate | |||||
| HEMPEL's Water-borne Epoxy Modified Finish 320 | Minimum | 20 h | 8 h | 4 h | 2½ h |
| Maximum | Extendable* | ||||
| Atmospheric, severe | |||||
| HEMPEL's Water-borne Epoxy Modified Finish 320 | Minimum | 30 h | 12 h | 6 h | 3½ h |
| Maximum | 35 days | 14 days | 7 days | 4½ days | |
Extendable* Depending on the actual exposure conditions, the coated surface may be recoated after an extended time. Contact your local Hempel representative for advice.
For products of the same generic chemical composition, recoat times are for reference only.
For further information, refer to Hempel's specifications.
- To achieve the stated drying times, adequate ventilation during application, drying and curing is essential.
| Ambient temperature | 25°C |
| Binder | 6 months |
| Curing agent | 6 months |
When stored in unopened original containers, shelf life is counted from the date of production. Thereafter, the product quality must be re-inspected. Storage at high temperatures may shorten the shelf life. For advice, consult Hempel.
- Store the product in accordance with the Safety Data Sheet, label and local regulations. Keep containers in a dry, cool, well-ventilated place away from heat and sources of ignition. Keep containers tightly closed. Handle with care.
| Number | Document description | Location/Notes |
| 3. | PDS | This document |
datasheet, which is also available for download at www.hempel.com.
| Dry Film Thickness | 1 µm | |
| GWP (Global Warming Potential) | 15.8 g CO₂e/m² |
Carbon footprint is based on a 1 µm dry film thickness formed over a surface area of 1 m².
The scope includes raw materials, transport to the Hempel factory, the Hempel production process, and any volatile organic compounds (VOC) emitted during and after use of the product.
Calculated based on the standard colours defined in this PDS. Values may vary with colour.
For further information, refer to the Hempel website (https://www.hempel.com/service-and-support/technical-guidelines) or your local Hempel website:
- Application methods - General application guide. This Product Data Sheet (“PDS”) relates to the product supplied (the “Product”), and its content is updated from time to time. Accordingly, the buyer/applicator should refer to the PDS supplied with the relevant batch of product (rather than an earlier version). In addition to the PDS, the buyer/applicator may receive some or all of the specifications, declarations and/or guides shown below, which are also available for download from the “Products” page of the Hempel website (www.hempel.com) (hereinafter the “Supplementary Documents”):
| 1. | Technical declaration | Provides one-off specific advice for the requirements of a specific project |
| 2. | Specifications | Issued for specific projects only |
| 4. | Explanatory notes to the PDS | Available for download at www.hempel.com, containing information related to product test parameters |
| 5. | Application guide | If available, provided at www.hempel.com |
| 6. | General technical guidelines (e.g. application and surface preparation) |
If the information in the PDS and the supplementary documents is inconsistent, the information shall take precedence in the order listed above. In this case, contact the Hempel representative for clarification. In addition, the buyer/applicator must give full consideration to the relevant safety information accompanying each product. Hempel accepts no liability for any defects arising from application not carried out fully in accordance with the recommendations and requirements of the relevant PDS and supplementary documents. The information and terms in this disclaimer apply to this PDS, the supplementary documents and any other relevant documents provided by Hempel for this product. In addition, unless otherwise expressly agreed in writing, supply of the product and all technical support are subject to Hempel's General Conditions of Sale, Delivery and Service.
Information is subject to the manufacturer's latest version; the manufacturer's latest TDS prevails.
The technical parameters on this page are taken from the product's original manufacturer technical datasheet, the copyright of which belongs to the manufacturer. If a rights holder considers the presentation inappropriate, contact us for verification and handling.
Packaging specifications and batch lead times are subject to actual availability. PleaseContact Uscontact us for project-based calculation.